- Macro1 (8 cm to 20 cm): an indication of early degradation of the top layer – ravelling, delamination, loose chippings, …
- Macro2 (20 cm to 60 cm): an indication of more advanced degradation of the top layer – cracks, potholes, …
- Mega1 (60 cm to 140 cm): unevenness that affects the driving experience – larger potholes, rutting, but also limited longitudinal undulations.
- Mega2 (140 cm to 3 m): larger unevenness – deep rutting, longer undulations, …
- Waviness (3 m to 5 m): longitudinal evenness over long distances, mainly relevant for roads driven at high speed.